Crinkle phenomenon of paint coat

Reasons:

1. Paint coat too thick;

2. Poor self-dry condition such as low temperature, high-humidity or over-ventilated.

3. Polluted air or poor-ventilated environment.

 

How to use:

1. Avoid spraying too thick;

2. Guarantee the fresh air and normal temperature and humidity in spraying environment.